This alloy has excellent strength and corrosion resistance, fair machining qualities and is hot headed and hot forged. Available in non-leaded C46400.
Standards | ASTM B 21, Temper H02 (1/2 Hard) |
UNS Designation Number | UNS C48500UNS C46400 |
Nominal Chemicals | C46400: Copper: 60.00%, Zinc: 39.25%, Tin 0.75%C48500: Copper: 60.00%, Zinc: 37.50%, Tin: 0.70%, Lead: 1.80% |
Stock Length | 12 ft |
Average Tensile Physical Properties | 70000 psi |
Average Yield Physical Properties | 27000 psi |
Average Elongation Physical Properties | 22 % |
Average Temper Physical Properties | As Extruded, About 1/2 Hard |
Features | LeadedNon-Leaded |
Extruded Material Size | 1 to 6.50 in |
Drawn Material Size | 0.078 to 2.50 in |