Aluminum bronze alloy C954 is used in a variety of applications for wear against steel or iron. Its resistance to wear is excellent. Recommended for high load, high wear situations. Used in wearplates, bushings, washers, gears & hold down screws.
Available in rounds & tube. Also cast to size as a centrifugal or sand cast
Specifications for C95400
ASTM | |
Rounds/tubes | ASTM B505 |
sand cast | ASTM B148 |
centrifugal | ASTM B271 |
All Methods | QQ-C390 |
Mechanical Properties for for C95400
tensile | yield | Elongation |
Brinell Hardness
|
|
centrifugal | 75K min. | 30K min. | 12% min. | 150 min. |
continuous cast | 85K min. | 32K min | 12% min. | |
sand cast | 75K min. | 30K min. | 12% min. | 150 min. |
Compositions for C95400 Aluminum Bronze
UNS No. | Copper | Iron | Nickel | Aluminum | Maganese |
C95400 | 83 | 3.0/5.0 | 1.5 max. | 10/11.5 | 0.50 max |
Physical Properties of C95400
Physical Properties
|
* As Cast, Field Strength 16 kA/m
|
** TQ 50 Temper, Field Sterngth 16 kA/m
|
Melting Point – Liquidus°F
|
1900 |
Melting Point – Solidus°F
|
1880 |
Densitylb/cu in. at 68°F
|
0.269 |
Specific Gravity
|
7.45 |
Electrical Conductivity% IACS at 68°F
|
13 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F
|
33.9 |
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)
|
9 |
Specific Heat CapacityBtu/ lb /°F at 68°F
|
0.1 |
Modulus of Elasticity in Tensionksi
|
15500 |
Magnetic Permeability*
|
1.27 |
Magnetic Permeability**
|
1.2 |
Applications for C95400 Aluminum Bronze
Bushings |
Bearings |
Wearplates
|
Impellers |
Pump Parts
|
Marine Products
|
ship building
|
worm gears
|
Hydraulic Press Main Liners
|
Worm Gears
|
Thrust Washers
|
TrunionBearings
|
Valve Seats
|
Valve Guides
|