This alloy has excellent strength and corrosion resistance, fair machining qualities and is hot headed and hot forged. Available in non-leaded C46400.

Standards ASTM B 21, Temper H02 (1/2 Hard)
UNS Designation Number UNS C48500UNS C46400
Nominal Chemicals C46400: Copper: 60.00%, Zinc: 39.25%, Tin 0.75%C48500: Copper: 60.00%, Zinc: 37.50%, Tin: 0.70%, Lead: 1.80%
Stock Length 12 ft
Average Tensile Physical Properties 70000 psi
Average Yield Physical Properties 27000 psi
Average Elongation Physical Properties 22 %
Average Temper Physical Properties As Extruded, About 1/2 Hard
Features LeadedNon-Leaded
Extruded Material Size 1 to 6.50 in
Drawn Material Size 0.078 to 2.50 in